Medición de retención de polímero de alto peso molecular en muestras de areniscas: berea, sandpack, usando trazadores químicos: Tritio, 2- FBOH y Variación de salinidad; con salmuera de 20 g/l

Mostrar el registro sencillo del ítem

dc.contributor.advisor Abrigo, Sergio es_ES
dc.contributor.other Estevez, Paola es_ES
dc.creator Jara, Leandro Agustín
dc.creator Malisani, Nicolas Agustin
dc.date 2025
dc.date.accessioned 2025-03-20T16:30:02Z
dc.date.available 2025-03-20T16:30:02Z
dc.identifier.uri https://rdi.uncoma.edu.ar/handle/uncomaid/18573
dc.description.abstract Este trabajo se realizó con el objetivo de cuantificar la retención de polímero de alto peso molecular en medios porosos (MP), específicamente en muestras de Berea y Sandpack. Además, se buscó caracterizar la aplicación de trazadores químicos alternativos al Tritio (HTO) comúnmente utilizado en ensayos de laboratorio. La retención de polímeros en el MP puede causar problemas técnicos y económicos, ya que parte del polímero inyectado no alcanza su destino debido al entrampamiento en los canales del MP y la adsorción en el mismo. Para abordar esta cuestión, se utilizó el polímero lineal FLOPAAM FP3630s, con un peso molecular de 18 MMDalton, y se evaluó el uso de un trazador salino y del trazador particionable 2-FBOH, en comparación con el trazador Tritio (HTO). Las muestras ensayadas incluyeron Berea y Sandpack, con permeabilidades del orden de 100 mD y 40 Darcy, respectivamente. Las muestras fueron saturadas con salmuera de salinidad 18 g/l. Se realizaron experimentos en el laboratorio de petrofísica de la Facultad de Ingeniería, Universidad Nacional del Comahue, La metodología incluyó la inyección de salmuera de salinidad 20 g/l, tritiada y aditivada con 2-FBOH, seguida de la inyección de una salmuera de salinidad de 18 g/l, para obtener curvas de variación de concentración de los trazadores. Se midió la salinidad con un equipo conductímetro, la concentración de tritio con un equipo de centelleo y la concentración de 2-FBOH con un espectrofotómetro UV-Vis. El análisis de los resultados permitió determinar el volumen poral de las muestras y calcular la cantidad de polímero retenido. Este estudio busca, además, optimizar futuros ensayos de laboratorio y proporcionar una alternativa viable al uso de trazadores radiactivos en la caracterización de medios porosos. es_ES
dc.description.abstract This study was conducted with the objective of quantifying the retention of high molecular weight polymer in porous media (PM), specifically in sandstone samples such as Berea and Sandpack. Additionally, it aimed to characterize the application of alternative chemical tracers to Tritium (HTO), which is commonly used in laboratory tests. Polymer retention in PM can cause technical and economic issues, as a portion of the injected polymer fails to reach its destination due to entrapment in the channels of the PM and adsorption within the porous medium. To address this issue, the linear polymer FLOPAAM FP3630s, with a molecular weight of 18 MMDalton, was used. The study evaluated the use of a saline tracer and the partitionable tracer 2-FBOH, in comparison to the Tritium (HTO) tracer. The tested samples included Berea and Sandpack sandstones, with permeabilities of approximately 100 mD and 40 Darcy, respectively. The samples were saturated with brine at a salinity of 18 g/L. Experiments were carried out in the petrophysics laboratory of the Faculty of Engineering at the National University of Comahue. The methodology included the injection of brine with a salinity of 20 g/L, enriched with tritium and 2-FBOH, followed by the injection of brine with a salinity of 18 g/L, to obtain concentration variation curves for the tracers. Salinity was measured using a conductivity meter, tritium concentration with a scintillation counter, and 2-FBOH concentration with a UV-Vis spectrophotometer. The analysis of the results allowed for the determination of the pore volume of the samples and the calculation of the amount of retained polymer. This study also seeks to optimize future laboratory tests and provide a viable alternative to the use of radioactive tracers in the characterization of porous media. es_ES
dc.format application/pdf es_ES
dc.publisher Universidad Nacional del Comahue. Facultad de Ingeniería es_ES
dc.rights Atribución-NoComercial-CompartirIgual 4.0 es_ES
dc.rights.uri https://creativecommons.org/licenses/by-nc-sa/4.0/ es_ES
dc.subject Retención de polímeros es_ES
dc.subject Trazadores quimicos es_ES
dc.subject Trazador 2-FBOH es_ES
dc.subject TRITIO (HTO) es_ES
dc.subject BEREA es_ES
dc.subject FLOPAAM FP3630S es_ES
dc.subject Adsorción es_ES
dc.subject Volumen poral es_ES
dc.subject Alternativas a trazadoresradioactivos es_ES
dc.subject Polymer retention es_ES
dc.subject Chemical tracers es_ES
dc.subject Tracer 2-FBOH es_ES
dc.subject Pore volume es_ES
dc.subject Alternative to radioactive tracers es_ES
dc.subject.other Ciencias Aplicadas es_ES
dc.title Medición de retención de polímero de alto peso molecular en muestras de areniscas: berea, sandpack, usando trazadores químicos: Tritio, 2- FBOH y Variación de salinidad; con salmuera de 20 g/l es_ES
dc.type proyecto de investigación es
dc.type other eu
dc.type acceptedVersion eu
unco.tesis.grado Licenciado en Ciencias Geológicas
dc.description.fil Fil: Jara, Leandro Agustín. Universidad Nacional del Comahue. Facultad de Ingeniería. Departamento de Geología y Petróleo; Argentina. es_ES
dc.description.fil Fil: Malisani, Nicolás Agustín. Universidad Nacional del Comahue. Facultad de Ingeniería. Departamento de Geología y Petróleo; Argentina. es_ES
dc.cole Trabajos Finales es_ES


Ficheros en el ítem

Este ítem aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del ítem

Atribución-NoComercial-CompartirIgual 4.0 Excepto si se señala otra cosa, la licencia del ítem se describe como Atribución-NoComercial-CompartirIgual 4.0